Most arguments about casting price come down to one line on the drawing: how tight the as-cast surfaces need to be.

CT6 is not the default

ISO 8062 CT6 is achievable in silica-sol investment casting at small sizes, but every grade tighter costs shell control, wax tooling accuracy and inspection time.

Machine what matters, cast the rest

Sealing faces, bores and threads belong to machining. Wall thickness, external profile and non-functional surfaces can stay at CT7–CT8 and save real money.

Leave enough stock

A 2 mm machining allowance on a 100 mm casting is normal; 0.5 mm invites a witness mark where the casting surface breaks through. Tell the foundry which surfaces will be machined.